3.18mm Eco-friendly Photopolymer flexo plate for Flexo Printing
Description
1)Excellent dot and isolated line reproduction
2)Solid printing performance
3)High latitude of exposure and processing
4)Good ink transfer
5)High impression
Technical Parameters :
Type | R-318 | |
Thickness(mm) | 3.18mm | |
Rigidity(Shore A) | 38-42 | |
Recommend relief depth(mm) | 0.9-1.5 | |
Image reproduction | 2%~95% | |
Maximum line line/inch | 120 | |
Minimum isolated line | 0.175mm (0.0068inch) | |
Minimum isolated dot | 0.25mm (0.01inch) | |
Suitable ink | Suitable for water and alcohol-based ink, incompatible with oil-based ink, hydrocarbon solvent or the ink containing ethyl acetate of more than 25% | |
Mainly applicable field | Corrugated board, thick board | |
Storage—raw plates | Unexposed plates should be stored in cool areas (4-32°C)away from heat. The plates must be placed flatly, and protected from contacting UV light. It is recommended to unpacked and handled in yellow light. | |
Storage—finished Plates | Printing plate should be avoid excessive white light, irradiating from sunlight and exposing in high concentrated ozone environments for a long time either. After being unloaded, the plates should be cleaned thoroughly. | |
Guarantee Period | Under the recommended storage condition, guarantee period of Flexographic Printing Plate is 24 months. | |
Packing (mm/inch) | 457×762 (18×30) | √ |
762×1016 (30×40) | √ | |
900×1200 (35.4×47.2) | √ | |
1067×1524 (42×60) | √ | |
1067×2032 (42×80) | √ | |
1200×2032 (47.2×80) | √ | |
1270×2032 (50×80) | √ |
Process parameters:
Type | R-318 | |
Thickness(mm) | 3.18mm | |
Back exposure(seconds) | 25-40 | |
Main exposure(seconds) | 7-20 | |
Rinsing(minutes) | 5-7 | |
Minimum drying time(hours) | 1.5-2 | |
Detackfying(minutes) | 5-7 | |
Post exposure(minutes) | 5 |
1)Platemaking conditions: modulator tube 80W(intensity in 365nm:9.7mW/cm2),Temperature of plate maker:24-30°C
2) All the parameters recommended above are all based on our platemaker,clients should adjust the data according to your own platermaker,power of ultraviolet lamp,depth of the files and other demands for the printing.Clients need to test on your machine.
Данные ресурс не является интернет-магазином, а лишь содержит ссылки на международную торговую площадку Alibaba.com