AIM Magnet Company manufacturing & sales of neodymium magnet for 12 years. We supply rare earth permanent magnetic products, focus on neodymium magnets & related magnetic products. NdFeB is called "permanent magnetic king", & is the strongest permanent material.
Customized Tiny Disc Permanent Magnet N52 China neodymium magnet D3x2mm
1. Material:Permanent Neodymium Magnet
2. Coating:Ni, NiCuNi (we all making three layers of plating,
Ni-Cu-Ni, plating thickness is 16-22μm(normal is 10-15μm) and Salt Spray testing time is 48h, that brighter and more antirust.
3. Certification: ISO9001-2008,REACH,ROHS
4. Testing: SST: 36~96 hours
5 working temperature:-40℃ ~80℃
6. Production time: 7 working days
7. Size Tolerance:+/-0.1mm
Description | Neodymium (NdFeB) Magnet | |||||||
Material | Sintered Neodymium-Iron-Boron | |||||||
Working Temperature | Grade | Max. Operating Temperature | Curie Temp. | |||||
N35-N52 | 80°C (176°F) | 310℃(590°F) | ||||||
33M- 48M | 100°C (212°F) | |||||||
33H-48H | 120°C (248°F) | |||||||
30SH-45SH | 150°C (302°F) | 320℃(608°F) | ||||||
30UH-40UH | 180°C (356°F) | 330℃(626°F) | ||||||
28EH-38EH | 200°C (392°F) | |||||||
28AH-35AH | 220°C (428°F) | 350℃(662°F) | ||||||
Electroplating | Surface | Coating | Thickness (Microns) | Color | ||||
Passivation | 0-1 | Silver Grey | ||||||
Nickel | Ni+Ni | 10-20 | Bright Silver | |||||
Ni+Cu+Ni | ||||||||
Zinc | Zn | 8-20 | Bright Blue | |||||
C-Zn | Shinny Color | |||||||
Tin | Ni+Cu+Sn | 15-20 | Silver | |||||
Gold | Ni+Cu+Au | 10-20 | Gold | |||||
Copper | Ni+Cu | 10-20 | Gold | |||||
Customized coating for Neodymium Magnet are available. | ||||||||
Note | 1.Be carefully fragile and clip hand. 2.Placed in a dry place,stored at suitable temperature. 3.Carefully draw them,close each other slowly and gently when connecting two magnets.Hard crushing cause magnet damage and cracks. |